Flow Loop Immersion Corrosion Testing

G2MT Labs offers single-phase liquid flow immersion corrosion testing and corrosion analysis that provides similar data to much larger systems but at a fraction of the cost, time, and effort. We have several standard practices we have developed, and our corrosion scientists will work with you to design the testing you need specifically for your application.

The laboratory currently operates 5 immersion corrosion testing flow loops that can run at temperatures from ambient up to 200 Degrees F in a wide range of liquids including oil, gas, water, mild acids, and more. We can accommodate multiple sample groups simultaneously in the same loop or keep each set of materials separate, based on your needs.

G2MT Labs Flow Loop Testing - Immersion Corrosion Analysis

G2MT Labs Flow Loop Testing – Immersion Corrosion Analysis in 3 loops

Capabilities:

  • Corrosion-resistant teflon-coated stainless steel vessels with high-temperature PVC connections
  • Temperature control and monitoring up from ambient temperature up to 200 Degrees F
  • Multiple ports for sample testing and analysis, can accomodate up to 18 samples per test loop
  • Dissolved oxygen monitoring port
  • pH monitoring port

We look forward to working with you! Please contact us today to get started or learn more about our flow loop corrosion analysis services.