Weld Qualification Procedure Development and Testing

Welding is the glue that holds modern industrial systems together. We understand the complexity, challenges, and corrosion issues that can occur, and are ready to help.  G2MT Labs’ experienced welding analysts and consultants can support you in the process of creating welding procedures and act as independent specialists for your welding analysis and consulting needs.

G2LabsWeb4

Welding Procedure Specification Development

The Welding Procedure Specification (WPS) is the formal document [1] describing the welding process and procedures. It is a guide to the welder for an accepted procedure that can repeatably achieve quality welds. A WPS is usually developed for each alloy and application. Our team of welders, M.S., and PhD metallurgists work with you to define a WPS for your process. If a process needs research for development, our analysis team will help you fine-tune your welding processes.

Weld Procedure Qualification Record (PQR) – Development and Testing

A WPQR is a company-specific qualification that is needed for each WPS [2]. It proves that the holding company possesses the technical welding knowledge necessary to perform metal joining work. Generally, a new welding procedure qualification record is required each time a welding procedure is introduced as part of the quality assurance process [3]. To obtain the qualification, an independent specialist must observe the new procedure being used on a sample welding plate or pipe.

Once the sample welding plate or pipe had been welded, it is cut into welding test samples, which can then be analyzed in our laboratories by destructive and non-destructive testing.

Weld non-destructive testing usually includes:

  • Visual Inspection,
  • X-ray,
  • Ultrasound Testing (UT),
  • Liquid penetrant (LP), and/or
  • magnetic testing procedures,

Weld destructive testing usually includes some combination of: Porosity in the root pass of a weld - G2MT Labs Houston

  • Tensile Testing,
  • Bend Testing,
  • Charpy Impact Testing,
  • Hardness Measurements,
  • Macro- and Microscopic Analysis
  • Ferrite Content Measurement,
  • CTOD, and/or
  • Corrosion Testing.

We then present the results of these tests in a certificate – the WPQR – which provides a practical assessment of the welding method description and verification that the weld passed the appropriate Weld Certification Tests per AWS and other standards body specifications.

G2MT Labs Weld Testing And Welding Consulting Services

G2MT Labs’ Houston welding laboratory is staffed with welding experts that are experienced in all aspects of welding and the requirements for ferrous/nonferrous properties, and polymer properties. We stay up-to-date with technological advancements in the welding industry and have dozens of welding-related publications in major journals and proceedings.

G2MT Labs provides the latest in welding testing and consulting services, including:

  • Welding process auditing,
  • Weld testing,
  • Weld qualification testing,
  • Weld failure analysis, and
  • Weld quality analysis.

Welding Standards and Specifications We Follow:

The welding experts at G2MT Labs have experience using a wide range of standards and codes including:

  • ASME B31.1, B31.3 (American Society of Mechanical Engineers Boiler and Pressure Vessel Code)
  • ISO 3834, 5817, 9606, 15609, 15614, NEN-EN (ISO Standards)
  • AWS D1.1 to AWS D1.6, AWS D9.1, AWS D14.1, AWS D14.6, AWS D15 (American Welding Society)
  • ASME Section IX QW-193 and others (ASME Section IX, Pressure & Power Piping Code)
  • AMS-STD-1595 Military & Aircraft, AMS-STD-2219  (Military Standards)
  • API 1104 Petroleum Piping Standard (American Petroleum Institute)
  • TÜV/PED 97/23/EC